Solid carbide drills surface
Solid carbide drills surface finishing by coatings
Solid carbide drills without surface finishing have quite good performance characteristics, which can be remarkably improved by providing them with a surface finishing by coating.
Therefore the nenok solid carbide drills are delivered with an especially powerful TiN coating or FIRE multi-layer coating.
TiN coating
- Titanium nitride coating is a thin wear-protection coating of golden yellow colour
- The single-layer titanium nitride coating is applied using the PVD method
- The hardness is 2300 HV
- The coating is suitable for a maximum application temperature of < 600 °C
FIRE coating
- The FIRE coating is a TiAlN/TiN multilayer coating in violet colour
- The hardness is 3300 HV
- The coating is suitable for a maximum application temperature of < 800 °C
Latest news

In a few days the time has come: The SteelDays at Behringer in Kirchhardt open their doors.The three-day OPENHOUSE is an important meeting place for the steel and metal processing industry, where…

Visit Nenok at the Steeldays Open House in Kirchardt, hosted by BehringerMay 9th to May 11th, 2023, Nenok will be making their Behringer Open House debut by exhibiting their used machinery and tool…

Das Nenok Team sendet einen herzlichen Weihnachtsgruß aus Köln und Langenargen.Wir wünschen allen Geschäftspartnern, Kunden und deren Mitarbeitern fröhliche und entspannte Weihnachtstage und einen…

Kaltenbach KBS620-KD615 system demonstration for sawing and drilling sectional steel.Nothing beats gathering practical impressions on site. This was also the opinion of the teachers of the 8th grade…